PolyLite™ASA是ABS的替代材料,具有更佳的耐候性。其抗紫外线性和卓越的机械性能使其成为户外应用的完美选择。PolyLite™ASA具有与PolyLite™ABS相同的机械和热性能,同时能够抵抗阳光(UV)和一般天气。其良好的耐候性使其成为需要经受自然环境的部件的理想选择。
Printing Temperature:
240˚C - 260˚C
Bed Temperature:
75˚C - 95˚C
Printing Speed:
30mm/s -50mm/s
Fan:
OFF
Direct Drive Retraction Distance:
1mm
Direct Drive Retraction Speed:
40mm/s
Indirect Drive Retraction Distance:
3mm
Indirect Drive Retraction Speed:
20mm
Drying Settings:
70˚C for 6h
Dry Settings Notes:
(Only if the material has absorbed moisture)